Lithium Ion Battery Raw Materials Lithium Chips for Coin Cell Materials 99.9

モデル番号.
2032

Typical Model
15.6*0.45

Silver Oxide Battery Model
Lithium Chips

LiMnO2 Battery Model
Lithium Chips

包装
Vacuum Package

アイテム
Lithium Chips

pH
(1% Solution)@25° C: >12

Boiling Point
1317° C

Melting Point
178° C (2%アル, 98%李)

外観
Silvery-White Soft Metal Solid

サイズ
15.6*0.25/15.6*0.45

Use
for Coin Cells

Supply 1
Lithium Ion Battery Materials

Supply 2
Lithium Ion Battery Equipment

パッケージ
100g/Tin

輸送パッケージ
Vacuumed Drum with Argon Filled

仕様
15.6*0.25/15.6*0.45

商標
gelon

Shandong China (Mainland)

生産能力
100トン/月

説明

>>>Lithium Aluminum Alloy Foil lithium plate(lithium chips):
外観: Silvery-white soft metal solid

PH: (1% solution)@25°C:>12

Boiling Point: 1317°C (Li metal with 1% すでに)

Melting Point: 180.5°C (Li metal with 1% すでに)

Solubility in water: Reacts violently with water

Specific Gravity: 0.5g/cc

Molecular Weight: 6.94

Copper current collector: 99.95min%

>>>5.1 Size and Chemical Composition(lithium chips)

Customizing according to customersrequirements.
1. Content: アル 0.1 ~ 5wt% Li balance
2. Size Width: 10 ~ 60 mm tolerance ± 0.5 mm
Thickness: 0.10 ~ 3.0 mm tolerance ± 0.01 mm

>>>5.2 包装(lithium chip):

Lithium foil with copper current collector is wound onto spools then dry packed under argon in hermetically sealed aluminized polyester pouches. Spool size is dependent on the dimensions and quantity of foil ordered .Please call for more details on packaging.

Lithium Ion Battery Raw Materials Lithium Chips for Coin Cell Materials 99.9

>>>5.3 Safety/Handling/Storage(lithium chips):

Complete information on product safety and handling is contained in the Material Safety Data Sheet .Always use good industrial hygiene when handling this product. Lithium foil with copper current collector reacts vigorously with water to give off corrosive lithium hydroxide and flammable hydrogen gas.

To maintain best quality, handle lithium foil with copper current collector under inert atmosphere of where relative humidity is maintained below 2%.

Lithium foil with copper current collector will meet the product specifications for six months from the date of shipment, provided the product is stored the original unadulterated package.
Lithium Ion Battery Raw Materials Lithium Chips for Coin Cell Materials 99.9

>>>5.4 Shipping Limitations(lithium chips):

Shipments of lithium foil with copper current collector are described asLithium, UN 1415,PG I.All shipments are Hazard Class 4.3 and requireDangerous when wetlabels.

Post, Parcel Not acceptable

Sea Class 4.3 (IMDG)

Road, Rail Class 4.3 11a (RID/ADR)

Air 15kg max. Cargo aircraft only

For shipments within Europe labeling for supply requirements are:

F Highly Flammable

C Corrosive

R&S phrases See Material Safety Data Sheet (MSDS)
Lithium Ion Battery Raw Materials Lithium Chips for Coin Cell Materials 99.9

We also can supply others:

1.)full set of lithium battery materials,含む :

LiMn2O4、LTO,LiNiMnCoO2(NMC),LiCoO2、グラファイト(MCMB)および他のカソード&負極電池材料;Alumimun foil,copper foil,lithium foil,バッテリーセパレーター,electrode,electrolyte,等.

2.)full set of lithium battery equipments,例えば:

混合機 –塗装機–オーブン–圧延機–溶接機–スリッティング / カットマシン –巻線機–sealing machineglove boxtesting machine,等.

3)full set of lithium battery technology.

実験室と生産ラインを設計できます,according to customer
Lithium Ion Battery Raw Materials Lithium Chips for Coin Cell Materials 99.9

Lithium Ion Battery Raw Materials Lithium Chips for Coin Cell Materials 99.9

>>>Any questions, pls contact us(lithium chips):